Search results
1751
[Page extract]
ASTM D413-98
ASTM D413 is a test method used to determine the force per unit width required to separate a rubber layer from a flexible substrate such as fabric, wire or sheet metal.
1752
[Page extract]
BS EN 12814-4
BS EN 12814-4 is a peel test method for testing welded joints of thermoplastics semi-finished products.
1753
[Page extract]
ISO 374-4
This document specifies the test method for the determination of the resistance of protective glove materials to degradation by dangerous chemicals with continuous contact.
1754
[Page extract]
Step-by-step procedure for reverse ratchet torque testing
Sample preparation
Condition the closures according to the specified standard to control environmental factors.
1755
[Page extract]
ASTM D575-91
These test methods cover two test procedures for determining the compression-deflection characteristics of rubber compounds other than those usually classified as hard rubber and sponge rubber.
1756
[Page extract]
BS ISO 7322
This International Standard specifies test methods for the determination of the following characteristics of composition cork (= product obtained from the agglutination of cork granules with the addition of a binder generally not derived from cork cells
1757
[Page extract]
ASTM D6742 / D6742M
ASTM D6742 is the standard test method for tensile and compression testing of filled-hole polymer matrix composite laminates. It provides instructions for modifying open-hole tension and compression test methods to determine filled-hole tensile and com
1758
[Page extract]
Prüfung des Drehmoments
Bei der Drehmomentprüfung wird ermittelt, wie ein Objekt reagiert, wenn es gedreht wird - im normalen Betrieb oder wenn es verdreht wird, bis es absichtlich versagt oder
1760
[Page extract]
BS EN 12242
The BS EN 12242 test method is used to determine the peel strength of a touch and close (also known as “hook and loop”) fastener through a 180° peel test that is able to determine average peel and the peel strength characteristics of the product for a g
1761
Case study
Prüfung der subkutanen Nadelschärfe
Beispiel für kundenspezifisches Engineering Hypodermische Nadeln werden getestet, um festzustellen, wie ihr Design die Leichtigkeit des Einführens in die Haut, die Schmerzen des Patienten und das Hauttrauma beeinflusst.
1762
[Page extract]
CETIE Guide 3
This guide is for producers of quality sparkling wines who carry out the secondary fermentation process in the bottle, also known as bottle fermentation.
1763
Case study
Getränkeflaschenträger aus Pappe aufklappbar
Beispiel für kundenspezifisches Engineering Ein Hersteller von vollständig geschlossenen Kartons wollte die Ausklappkraft für eine Vielzahl von Designs testen, die hauptsächlich zum Verpacken von Getränkeflaschen und Dosen verwendet wurden.
1764
[Page extract]
ISO 9664
The principle of the method specified is cyclically stressing the specimen in a way that may be regarded as the superposition of an alternating stress on a static stress which is the mean stress.
1765
[Page extract]
ASTM D1621
ASTM D1621 is used to measure the compressive properties of rigid cellular materials, particularly expanded plastics. Calculations include compressive strength, compressive strain, compressive stress and compressive modulus.
1766
Case study
Schältests von vakuumgeformten Behältern
Beispiel für kundenspezifisches Engineering Halbstarre thermogeformte Verpackungen, die mit Folie oder Folie versiegelt sind, werden üblicherweise nach der "45-Grad-Schälmethode" getestet.
1767
[Page extract]
BS EN 12568
Protective footwear, Protective clothing, Toe-caps, Metals, Non-metals, Impact strength, Performance testing, Dimensions, Length, Impact testing, Compression testing, Penetration tests, Corrosion resistance, Corrosion tests, Bend testing, Marking, Test
1768
[Page extract]
ASTM D790-17
ASTM D790 is used to determine the flexural properties of unreinforced and reinforced plastics, including high modulus composites and electrical insulating materials utilizing a three-point loading system to apply a load to a simply supported beam (spec
1769
[Page extract]
ASTM D2918
This test method provides data for assessing the durabilities of adhesive joints by means of T-peel type specimens stressed in contact with air, air in equilibrium with certain solutions, water, aqueous solutions, or other environments at various temper
1770
Case study
Smoke grenade canister integrity
Customised engineering example
A manufacturer of smoke grenades required a means of testing the cap pull-off strength. The particular challenge was to grip the smooth metal cylinder for up to 5 kN of pulling force.
1771
[Page extract]
ASTM D5635-11
An important factor affecting the performance of membrane roofing systems is their ability to resist dynamic puncture loads. This test method provides a means to assess dynamic puncture resistance.
1772
[Page extract]
ASTM D5467 / D5467M-97
ASTM D5467 is a test method that determines the in-plane compressive properties of polymer matrix composite materials reinforced by high-modulus fibers in a sandwich beam configuration.
1773
Event
Automotive Component Torque Testing
This webinar will focus on the measurement of the torque resistance in knobs, switches, and torsion springs, which are among several components in automobiles that require testing to ensure quality, performance, and safety.
1774
Case study
Betätigungskraft des Pumpspenders
Anforderung Der Kunde stellt eine Reihe von Dosierpumpen für die Kosmetik- und Schönheitspflegeindustrie her. Es wurde eine Anforderung zum Messen der Betätigungskraft der Pumpenbaugruppe und der Abziehkraft des Pumpengriffs ermittelt.