Search results
1751
[Page extract]
BS EN ISO 80369-20
These standards describes the methods for testing the performance of 6% Luer lock fittings including assembly, leak tightness, stress cracking, and separation force.
1752
[Page extract]
ISO 12625-4
Specifies a test method for the determination of the tensile strength, stretch at break and tensile energy absorption of tissue paper and tissue products. It uses a tensile-testing apparatus operating with a constant rate of elongation.
1753
[Page extract]
ASTM D7084-04
1.1 This test method covers the determination of bulk crush strength of a bed of formed catalyst particles 1⁄32 to 3⁄16 in.
1754
[Page extract]
ISO 34-1
ISO 34-1 measures tear strength test methods for rubber test samples. The test results in measurement of a materials resistance to tearing. Tear strength can also be used to monitor material anisotropy of a material.
1755
[Page extract]
ASTM C907
This test method covers a laboratory procedure for determining the tensile adhesive strength of a preformed tape sealant. The type of failure can be determined, and the degree of cohesive/adhesive failure can be estimated.
1756
[Page extract]
ASTM C364
This test method covers the compressive properties of structural sandwich construction in a direction parallel to the sandwich facing plane.
1757
[Page extract]
BS EN 14372
This document establishes minimum safety requirements and specifies appropriate test methods for children’s cutlery and feeding utensils designed for the use of children aged up to 3 years, with or without parental supervision.
1758
Specials
Extensometry low-force
Extensometer ready
Mecmesin's MultiTest-dV range supports extensometry in your testing methods when configured to run VectorPro™ MT materials testing software.
1759
[Page extract]
TAPPI T 807
This method describes a procedure for measuring the bursting strength of linerboard using a disk shaped diaphragm. Basis weights for this method should be 98 g/m (20#/MSF) and higher. The minimum burst should be 350 kPa (51 psi).
1760
[Page extract]
ASTM D4533-11
This test method is an index test used to measure the force required to continue or propagate a tear in woven or non-woven geotextiles by the trapezoid method.
1761
[Page extract]
BS EN 863
Protective clothing, Clothing, Perforating tests, Penetration tests, Mechanical testing, Tensile testing, Test equipment, Specimen preparation, Performance testing
1762
[Page extract]
BS EN 1263-1
Safety nets, Restraint systems (protective), Construction equipment, Safety devices, Building sites, Occupational safety, Performance, Man-made fibres, Polyamide fibres, Polyolefin fibres, Ropes, Performance testing, Mechanical testing, Tensile testing,
1763
[Page extract]
BS EN ISO 6892-1
This part of ISO 6892 specifies the method for tensile testing of metallic materials and defines the mechanical properties which can be determined at room temperature.
1764
[Page extract]
ASTM D3469
These test methods measure the downward forces during the disengagement of lug-style caps from their respective containers. The methods measure the maximum torque developed while the cap is further disengaged by turning of the container.
1765
[Page extract]
ASTM D7269/D7269M-11
These test methods cover the tensile testing of aramid yarns, cords twisted from such yarns, and fabrics woven from such cords.
1766
Specials
UTM FAQs
FAQs
How does the OmniTest universal testing machine compare in size and portability?
The OmniTest universal testing machine (UTM) offer
1767
[Page extract]
ISO 20502
SO 20502:2005 describes a method of testing ceramic coatings by scratching with a diamond stylus.
1768
[Page extract]
BS EN 681-1
This standard specifies requirements for materials used in vulcanized rubber seals for:
1) cold potable water supply (up to 50®C);
1769
[Page extract]
ASTM D4776 / D4776M-18
ASTM D4776 is a test method used to determine the maximum adhesion force of tyre cords in rubber compounds.
1770
[Page extract]
ASTM F152-95
ASTM F152 is a test standard that covers tensile strength of nonmetallic gasketing materials at room temperature.
1771
Event
Needle Sharpness & Puncture Resistance Testing
Hypodermic needles are tested to determine how their design influences the ease of insertion into the skin, patient pain and skin trauma.
1772
[Page extract]
EEC 2006/42/EC
The Directive 2006/42/EC of the European Parliament and of the Council of 17 May 2006 is a European Union directive concerning machinery and certain parts of machinery.[1] Its main intent is to ensure a common safety level in machinery placed on the mar
1773
[Page extract]
ASTM D876 - 13
ASTM D876 is a test method covering the testing of general-purpose (Grade A), low-temperature (Grade B), and high-temperature (Grade C)2 non-rigid vinyl chloride polymer tubing, or its copolymers with other materials, for use as electrical insulation.
1774
[Page extract]
ISO 34-2
ISO 34-2 specifies a method for the determination of the tear strength of small test pieces (Delft test pieces) of vulcanized or thermoplastic rubber.