Search results
1953
[Page extract]
ASTM D1995
These test methods cover procedures by which autohesives can be tested in four commonly practiced stressing modes, namely: compression shear, cleavage, climbing drum peel, and T-peel, and in various combinations of rigid-to-rigid, flexible-to-rigid, and
1954
Caso de estudio
Pruebas de extracción de tapones de whisky.
Requisito Para mejorar la calidad y el almacenamiento de su producto premium de $ 1000, el equipo de I + D de un fabricante de whisky escocés líder necesitaba optimizar el diseño de sus tapones de botellas.
1955
[Page extract]
ISO 7886-4
This document specifies requirements for sterile single-use hypodermic syringes made of plastic and rubber materials with or without needle, and intended for the aspiration of fluids or for the injection of fluids immediately after filling and of design
1956
[Page extract]
ASTM C203
ASTM C203 is a test method that covers the determination of the breaking load and calculated flexural strength of a rectangular cross section of a preformed block-type thermal insulation tested as a simple beam.
1957
[Page extract]
ASTM D7137 / D7137M-17
ASTM D7137 is a test method that measures the compression residual strength properties of multidirectional polymer matrix composite laminated plates, which have been subjected to quasi-static indentation
1958
[Page extract]
SAE J174
This test procedure is intended to provide a quality control method for checking torque-tension characteristics of non-prevailing torque type threaded steel fasteners 1/4 through 1 in nomial diameters.
1959
[Page extract]
Key standards in compressive deformation testing
Compliance with recognised standards ensures that results are accurate, repeatable, and accepted by regulatory bodies. Examples include:
1960
[Page extract]
Introduction to elongation and recovery testing
In industries working with textiles, rubber, elastomers, and flexible plastics, these properties are directly linked to product reli
1961
[Page extract]
ISO 1798
ISO 1798 specifies a method for determining the strength and deformation properties of flexible cellular materials when a test piece is extended at a constant rate until it breaks.
This test standard is equivalent to BS EN ISO 1798:2008
1962
[Page extract]
ISO 505
ISO 505 specifies a method of test for the measurement of the propagation resistance of an initial tear in textile conveyor belts, either in full thickness or of the carcass only.
1963
[Page extract]
ASTM D2979
This test method covers measurement of the pressure-sensitive tack of adhesives.
1965
[Page extract]
ISO 813
ISO 813 specifies a method for the determination of the adhesive strength of a vulcanized or thermoplastic rubber bonded to a rigid substrate, using a test piece comprising a strip of rubber bonded to a single plate of rigid material.
1966
[Page extract]
ASTM D1871
This test method is used to test the strength of adhesion of single-filament wire to vulcanized rubber compounds. It applies to wire made from brass, bronze or zinc coated steel wire.
1967
[Page extract]
ISO 12625-4
Specifies a test method for the determination of the tensile strength, stretch at break and tensile energy absorption of tissue paper and tissue products. It uses a tensile-testing apparatus operating with a constant rate of elongation.
1968
[Page extract]
ASTM D380
ASTM D380 is a set of test methods for determining testing and inspection procedures for rubber hoses e.g. hydraulic hoses and automotive hoses.
1969
[Page extract]
ISO 11339
ISO 11339:2010 specifies a T‑peel test for the determination of the peel strength of an adhesive by measuring the peeling force of a T‑shaped bonded assembly of two flexible adherends. This test procedure does not provide design information.
1970
Specials
Thermal cabinet environment chamber
Environmental chamber capability
Mecmesin's OmniTest twin column range can accommodate an environmental chamber to test materials in controlled ambient conditions.
1971
[Page extract]
ASTM D2659
ASTM D2659 determines the mechanical properties of blown thermoplastic containers under columnar crush conditions at a steady rate of compression. Any container, whether blown commercially or in the laboratory, may be used as the test specimen.
1972
[Page extract]
BS EN ISO 10619-1
BS EN ISO 10619-1 is a test method covering bending tests on rubber or plastics hoses and tubing.
1973
[Page extract]
BS EN 1464
Specifies a floating roller method for the determination of the peel resistance of adhesive bonds between one rigid adherend and one flexible adherend when tested under specified conditions of preparation and testing.
1974
Caso de estudio
Prueba de primavera estabilizada
Ejemplo de ingeniería personalizada Nuestro cliente necesitaba probar una serie de muelles pequeños y livianos bajo compresión. Para evitar el pandeo y el movimiento lateral de los resortes, se requería un eje de soporte o una varilla guía.
1975
[Page extract]
TAPPI T 818