Search results
1951
[Page extract]
ASTM F1566-09
These test methods cover recognized methods for testing mattress innersprings, boxsprings, and finished mattresses or mattress sets, or both, to ensure uniformity of results.
1952
[Page extract]
ASTM D7617/D7617M-11
This test method specifies the test requirements for (FRP) composite smooth round rods and textured bars for determining the transverse shear strength via a double shear fixture.
1953
[Page extract]
ASTM D2979
This test method covers measurement of the pressure-sensitive tack of adhesives.
1954
[Page extract]
Benefits and limitations of compressive shear testing
Advantages
High precision - accurate measurement of shear strength under controlled compression
<
1955
[Page extract]
ASTM D2148
ASTM D2148 is a test standard that for testing bondable silicone rubber tapes, which form a sealed structure either with the application of heat (and pressure if needed) or by the process of auto-adhesion (self-fusing).
1956
[Page extract]
ASTM D3807
ASTM D3807 is a test method used to determine the strength properties of adhesives in cleavage peel by tension loading. It allows the comparative testing of cleavage/peel strengths of bonded engineering thermoplastic adherends.
1957
[Page extract]
ISO 8510-1
Particularly suitable for use with less flexible adherends for which a 180 ° peel test is not suitable because the adherends crack, break or delaminate. A bonded assembly of two adherends is prepared using the adhesive under test.
1958
[Page extract]
BS EN 1393
BS EN 1393 specifies a test method for testing the longitudinal tensile properties of glass-reinforced thermosetting plastics (GRP) pipes.
1959
[Page extract]
BS EN ISO 8670-2
Two part test on filled bags:
1) 20 N tensile flange seal test, pulled in two directions in turn, at 180 degrees, in shear plane across flange, bag held by transparent custom plate
1960
[Page extract]
ISO 594-2
ISO 594 and EN 1707 contain 8 separate tests, some of which are only applicable to Luer lock fittings. Most of these tests require that the sample be assembled to a particular precision steel reference fitting.
1961
[Page extract]
ASTM E8/E8M-13a
These test methods cover the tension testing of metallic materials in any form at room temperature, specifically, the methods of determination of yield strength, yield point elongation, tensile strength, elongation, and reduction of area.
1962
[Page extract]
PSTC 8
Unwind adhesion is a quantitative measure of the degree of ease or difficulty in unwinding a roll of tape.
The test specimen shall be any 10 m (10 yard) or more roll of pressure sensitive tape - preferably 24 mm (1”) wide.
1963
Caso de estudio
Prueba de primavera estabilizada
Ejemplo de ingeniería personalizada Nuestro cliente necesitaba probar una serie de muelles pequeños y livianos bajo compresión. Para evitar el pandeo y el movimiento lateral de los resortes, se requería un eje de soporte o una varilla guía.
1964
[Page extract]
TAPPI T 818
The ring crush test correlates with edgewise compression strength of paperboard. This method is intended for paperbaord between 0.28mm (0.011 in.) and 0.51mm (0.020 in) thick.
1965
[Page extract]
ASTM E1820-18ae1
The ASTM E1820 test method covers procedures and guidelines for the determination of fracture toughness of metallic materials using the following parameters: K, J, and CTOD (δ). Toughness can be measured in the R-curve format or as a point value.
1966
[Page extract]
ASTM D3410 / D3410M
ASTM D3410 determines the compressive properties of polymer matrix composite materials reinforced by high-modulus fibers.
1967
[Page extract]
ASTM D5169-98
This test method measures the shear strength of hook and loop touch fasteners using a recording constant rate of extension (CRE) tensile testing machine.
1968
[Page extract]
BS EN 520
Plasterboard, Gypsum plaster, Boards, Wall linings, Construction systems parts, Performance, Strength of materials, Fire resistance, Sound insulation, Water vapour, Permeability, Thermal resistance, Performance testing, Dimensional measurement, Physical
1969
[Page extract]
ISO 7810
Stipulates test method as per ISO/IEC 10373-1 for determining the Peel Strength of cards.
1970
Specials
Thermal cabinet environment chamber
Environmental chamber capability
Mecmesin's OmniTest twin column range can accommodate an environmental chamber to test materials in controlled ambient conditions.
1972
[Page extract]
BS EN 1464
Specifies a floating roller method for the determination of the peel resistance of adhesive bonds between one rigid adherend and one flexible adherend when tested under specified conditions of preparation and testing.
1973
[Page extract]
ASTM B913
This test method establishes the requirements for a standardized method of evaluating the quality of crimped-type electrical connections to solid or stranded conductors.
1974
[Page extract]
IEC 61196-1-308