Search results
1951
[Page extract]
ASTM F1147-05
This test method covers tension testing of calcium phosphate and metallic porous coatings adhering to dense metal substrates at ambient temperatures.
1952
[Page extract]
Key standards in compressive deformation testing
Compliance with recognised standards ensures that results are accurate, repeatable, and accepted by regulatory bodies. Examples include:
1953
[Page extract]
Introduction to elongation and recovery testing
In industries working with textiles, rubber, elastomers, and flexible plastics, these properties are directly linked to product reli
1954
[Page extract]
ASTM E8/E8M-13a
These test methods cover the tension testing of metallic materials in any form at room temperature, specifically, the methods of determination of yield strength, yield point elongation, tensile strength, elongation, and reduction of area.
1955
[Page extract]
SAE J174
This test procedure is intended to provide a quality control method for checking torque-tension characteristics of non-prevailing torque type threaded steel fasteners 1/4 through 1 in nomial diameters.
1956
[Page extract]
BS EN 1719
Adhesives, Adhesive strength, Adhesion tests, Paper, Board (paper), Pressure-sensitive materials, Testing conditions, Mathematical calculations
1957
[Page extract]
ISO 1798
ISO 1798 specifies a method for determining the strength and deformation properties of flexible cellular materials when a test piece is extended at a constant rate until it breaks.
This test standard is equivalent to BS EN ISO 1798:2008
1958
[Page extract]
Benefits and limitations of compressive shear testing
Advantages
High precision - accurate measurement of shear strength under controlled compression
<
1959
[Page extract]
ASTM D3914
ASTM D3914 is a test method used to measure the in-plane shear strength of pultruded, glass-fiber reinforced, thermosetting plastic rod in diameters ranging from 19 to 32 mm.
1960
[Page extract]
ISO 505
ISO 505 specifies a method of test for the measurement of the propagation resistance of an initial tear in textile conveyor belts, either in full thickness or of the carcass only.
1961
[Page extract]
ASTM F1566-09
These test methods cover recognized methods for testing mattress innersprings, boxsprings, and finished mattresses or mattress sets, or both, to ensure uniformity of results.
1962
[Page extract]
ASTM D7617/D7617M-11
This test method specifies the test requirements for (FRP) composite smooth round rods and textured bars for determining the transverse shear strength via a double shear fixture.
1963
Specials
Thermal cabinet environment chamber
Environmental chamber capability
Mecmesin's OmniTest twin column range can accommodate an environmental chamber to test materials in controlled ambient conditions.
1964
[Page extract]
ISO 12625-4
Specifies a test method for the determination of the tensile strength, stretch at break and tensile energy absorption of tissue paper and tissue products. It uses a tensile-testing apparatus operating with a constant rate of elongation.
1965
[Page extract]
ISO 7810
Stipulates test method as per ISO/IEC 10373-1 for determining the Peel Strength of cards.
1966
[Page extract]
ISO 11339
ISO 11339:2010 specifies a T‑peel test for the determination of the peel strength of an adhesive by measuring the peeling force of a T‑shaped bonded assembly of two flexible adherends. This test procedure does not provide design information.
1967
[Page extract]
TAPPI T 818
The ring crush test correlates with edgewise compression strength of paperboard. This method is intended for paperbaord between 0.28mm (0.011 in.) and 0.51mm (0.020 in) thick.
1968
[Page extract]
ASTM B913
This test method establishes the requirements for a standardized method of evaluating the quality of crimped-type electrical connections to solid or stranded conductors.
1969
[Page extract]
ASTM E1820-18ae1
The ASTM E1820 test method covers procedures and guidelines for the determination of fracture toughness of metallic materials using the following parameters: K, J, and CTOD (δ). Toughness can be measured in the R-curve format or as a point value.
1970
Event
Wine & Spirits Capping: Cork Pull & Twist Caps
Wine packaging has a great influence on the quality of the product delivered to the customer.
1972
[Page extract]
ISO 813
ISO 813 specifies a method for the determination of the adhesive strength of a vulcanized or thermoplastic rubber bonded to a rigid substrate, using a test piece comprising a strip of rubber bonded to a single plate of rigid material.
1973
[Page extract]
ASTM D5169-98
This test method measures the shear strength of hook and loop touch fasteners using a recording constant rate of extension (CRE) tensile testing machine.
1974
[Page extract]
BS EN 520
Plasterboard, Gypsum plaster, Boards, Wall linings, Construction systems parts, Performance, Strength of materials, Fire resistance, Sound insulation, Water vapour, Permeability, Thermal resistance, Performance testing, Dimensional measurement, Physical
1975
[Page extract]
ASTM D1871
This test method is used to test the strength of adhesion of single-filament wire to vulcanized rubber compounds. It applies to wire made from brass, bronze or zinc coated steel wire.